2767 MOULD STEEL

 

 

APPLICATIONS

Plastic moulding dies, zinc diecasting dies, extrusion die holders and press components, engineering components requiring high strength. 

 

ANNEALING

Heat slowly to 630°C / 650°C, soak thoroughly for six hours and furnace cool.  The usual annealed hardness is up to 285 HB.