ASP 2030 HIGH-SPEED STEEL
| COMPOSITION % |
C | Cr | Mo | W | V | Co | |
| 1.28 | 4.20 | 5.0 | 6.40 | 3.10 | 8.50 | ||
| STANDARDS |
SS 2726 |
||||||
| CONDITION AS SUPPLIED | Soft annealed | max 300 HB | |||||
| Drawn | max 320 HB | ||||||
|
|
||
|
ASP 2030 is a high-alloy high-speed steels that contains cobalt
(Co). It is manufactured powder-metallurgically using the ASP
process. The steel is atomized, compacted and processed to the
dimensions required. The result is an extremely homogeneous steel
with a unique combination of properties. ASP 2030's homogeneous structure enhances such properties as dimensional stability and shape stability during heat treatment, as well as improving grindability and toughness. Toughness is good even for large dimensions. ASP 2030's method of manufacture and composition mean that it can provide high hot hardness and good wear resistance. |